Knowledge

Reasons for uneven thickness of non-woven fabric in production process

Nov 01, 2021 Leave a message

1. Uneven cotton mixing of low melting point fiber and conventional fiber: because different fibers have different cohesion, generally speaking, low melting point fiber has greater cohesion than conventional fiber. If the low melting point fiber is unevenly dispersed, the part with less content cannot form sufficient network structure in time, so the produced non-woven fabric is thin, Compared with the low melting point, the place with more fiber content forms a thicker situation.

2. Incomplete melting of low melting point fiber: this situation is mainly due to insufficient temperature. For non-woven fabrics with low base weight, it is not easy to have insufficient temperature, but special attention should be paid to products with high base weight and high thickness. For example, the non-woven fabric on the edge is usually thicker because it has enough heat. The non-woven fabric in the middle part is easy to form a thinner non-woven fabric because of insufficient heat, which is also one of the reasons.

3. High shrinkage of fiber: whether conventional fiber or low melting point fiber, if the hot air shrinkage of fiber is high, uneven thickness will also occur during the production of non-woven fabric.

What are the reasons for the static electricity generated during the production of non-woven fabrics?

1. External factors may be that the weather is too dry and the humidity is not enough.

2. When there is no antistatic agent on the fiber, because the moisture regain of polyester cotton is 0.3%, it is easy to generate static electricity during the production of non-woven fabric due to the lack of antistatic agent.

3. The oil content of the fiber is low, and the relatively low content of electrostatic agent will also produce static electricity.

4. The method to prevent static electricity is not only to humidify the production workshop, but also to effectively eliminate oil-free cotton in the cotton feeding stage.

What are the reasons for the uneven hardness and softness of non-woven fabrics under the same processing conditions?

1. Due to the uneven cotton mixing of low melting point fiber and conventional fiber, the part with high content of low melting point is harder, on the contrary, the part with low content is softer.

2. In addition, incomplete melting of low melting point fibers can easily lead to soft non-woven fabrics.

3. The high shrinkage of fiber will also cause the problem of uneven soft and hard of non-woven fabric.

Send Inquiry